A672 J90 EFW Straight Welded Pipe
A672 J90 EFW pipe Description
A672 J90 is a carbon or low alloy steel electrofusion welded pipe for use in medium, high temperature and high pressure fluid transfer systems.
J90: Indicates a minimum yield strength of 90 ksi (approximately 620 MPa), which is a high yield strength grade that requires alloying elements or heat treatment to enhance properties.
Carbon (C Less than or equal to {{0}}.30%), manganese (Mn Less than or equal to 1.65%), silicon (Si 0.15% ~ 0.40%) is the main to meet the basic strength requirements
Normalising (CL12): Refine the grain and improve the toughness;
Normalising + tempering (CL22/CL32): balancing strength and low-temperature impact toughness, suitable for high pressure scenarios.
Welding technology: Electrofusion welding (EFW) or double-sided submerged arc welding (SAWL) to ensure that the strength of the weld is consistent with that of the base material.
A672 J90 EFW Welding Pipe Specification
|
A672 J90 Welded pipe/spiral pipe |
|
|
API, SNI, JIS, ISO9001 |
|
|
±1% |
|
|
7~15days or spots |
|
|
1mm~150mm |
|
|
19mm~2600mm |
|
|
5.8m~12m or To meet customer's demand |
|
| A45,A50,A55,B55,B60,B65,B70,C55,C60,C65,C70,D70,D80,E55,E60,H75,H80,J80,J90,J100,L65,L70,L75,N75 | |
A672 J90 EFW SAW pipe



A: We are a factory and one of the famous line pipe manufacturers in China. Our headquarter is located in Henan, China, since 2008.
A: 30 tonnes.
Популярни тагове: a672 j90 efw straight welded pipe, China a672 j90 efw straight welded pipe manufacturers, suppliers, Електрофузионна заварена въглеродна стоманена тръба, Закупете електрофузионна заварена тръба, Безпроблемни механични тръби, Рекламна електрофузионна заварена тръба, Заварена тръба за онлайн пазар на пазара, ASTM A672 степен B60 C65 EFW стоманена тръба